AUSTENITIC STAINLESS STEEL AND SPRING

An austenitic stainless steel consists of 0.010 to 0.200% by mass of C, 2.00% by mass or less of Si, 3.00% by mass or less of Mn, 0.035% by mass or less of P, 0.0300% by mass or less of S, 6.00 to 14.00% by mass of Ni, 20.0 to 26.0% by mass of Cr, 3.00% by mass or less of Mo, 0.01 to 3.00% by mass o...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: SEKIMUKAI, Kotaro, IMAKAWA, Kazunari
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:An austenitic stainless steel consists of 0.010 to 0.200% by mass of C, 2.00% by mass or less of Si, 3.00% by mass or less of Mn, 0.035% by mass or less of P, 0.0300% by mass or less of S, 6.00 to 14.00% by mass of Ni, 20.0 to 26.0% by mass of Cr, 3.00% by mass or less of Mo, 0.01 to 3.00% by mass of Cu, 1.000% by mass of less of Ti, 0.200% by mass or less of Al, 0.1000% by mass or less of Ca, 0.100 to 0.250% by mass of N, and 0.0080% by mass or less of 0, the balance being Fe and impurities.