Sulfide Solid Electrolyte
A sulfide solid electrolyte is provided having peak A at 2θ=20.7°±0.5° in an X-ray diffraction pattern obtained by performing X-ray diffraction measurement using CuKα1 radiation. It is preferable that the sulfide solid electrolyte has peak B at 2θ=25.4°±1.0° in the X-ray diffraction pattern obtained...
Gespeichert in:
Hauptverfasser: | , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | A sulfide solid electrolyte is provided having peak A at 2θ=20.7°±0.5° in an X-ray diffraction pattern obtained by performing X-ray diffraction measurement using CuKα1 radiation. It is preferable that the sulfide solid electrolyte has peak B at 2θ=25.4°±1.0° in the X-ray diffraction pattern obtained by performing X-ray diffraction measurement using CuKα1 radiation. It is also preferable that the value of the ratio of IA to IB, IA/IB, is more than 0 and 0.7 or less, where IA is the intensity of peak A and IB is the intensity of peak B. It is also preferable that the sulfide solid electrolyte has peak C at 2θ=22.0°±0.5° in the X-ray diffraction pattern obtained by performing X-ray diffraction measurement using CuKα1 radiation. |
---|