STABLE HIGH CONDUCTIVITY OXIDE ELECTROLYTE
The present invention relates to rhomboidal phase bismuth oxide that maintains electric conductivity of at least about 1×10−2 S/cm at temperature of about 500° C. for at least about 100 hours. In particular, the bismuth oxides of the invention have stable conductivity at a temperature range from abo...
Gespeichert in:
Hauptverfasser: | , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | The present invention relates to rhomboidal phase bismuth oxide that maintains electric conductivity of at least about 1×10−2 S/cm at temperature of about 500° C. for at least about 100 hours. In particular, the bismuth oxides of the invention have stable conductivity at a temperature range from about 500° C. to about 550° C. |
---|