FORMULATIONS FOR HIGH POROSITY CHEMICAL MECHANICAL POLISHING PADS WITH HIGH HARDNESS AND CMP PADS MADE THEREWITH
The present invention provides CMP polishing pads or layers having a Shore DO (15 second) hardness of from 40 to 80 made from a two-component reaction mixture of (i) a liquid aromatic isocyanate component comprising one or more aromatic diisocyanates or a linear aromatic isocyanate-terminated uretha...
Gespeichert in:
Hauptverfasser: | , , , , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | The present invention provides CMP polishing pads or layers having a Shore DO (15 second) hardness of from 40 to 80 made from a two-component reaction mixture of (i) a liquid aromatic isocyanate component comprising one or more aromatic diisocyanates or a linear aromatic isocyanate-terminated urethane prepolymer, and (ii) a liquid polyol component comprising a) one or more polymeric polyols, b) from 15 to 36 wt. %, based on the total weight of the liquid polyol component, of one or more small chain difunctional polyols having from 2 to 6 carbon atoms, c) from 0 to 25 wt. %, based on the total weight of the liquid polyol component, of a liquid aromatic diamine which is a liquid at standard pressure and at 40° C., and d) an amount of water or CO2-amine adduct sufficient to reduce the density of a CMP polishing pad made from the two-component reaction mixture to from 0.2 to 0.50 g/mL, wherein the reaction mixture comprises 60 to 75 wt. % of hard segment materials, based on the total weight of the reaction mixture. |
---|