A sulfide solid electrolyte is provided having peak A at 2θ=20.7°±0.5° in an X-ray diffraction pattern obtained by performing X-ray diffraction measurement using CuKα1 radiation. It is preferable that the sulfide solid electrolyte has peak B at 2θ=25.4°±1.0° in the X-ray diffraction pattern obtained...