SULFIDE SOLID ELECTROLYTE

A sulfide solid electrolyte is provided having peak A at 2θ=20.7°±0.5° in an X-ray diffraction pattern obtained by performing X-ray diffraction measurement using CuKα1 radiation. It is preferable that the sulfide solid electrolyte has peak B at 2θ=25.4°±1.0° in the X-ray diffraction pattern obtained...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: TAKAHASHI, Tsukasa, CHIKUMOTO, Takashi
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:A sulfide solid electrolyte is provided having peak A at 2θ=20.7°±0.5° in an X-ray diffraction pattern obtained by performing X-ray diffraction measurement using CuKα1 radiation. It is preferable that the sulfide solid electrolyte has peak B at 2θ=25.4°±1.0° in the X-ray diffraction pattern obtained by performing X-ray diffraction measurement using CuKα1 radiation. It is also preferable that the value of the ratio of IA to IB, IA/IB, is more than 0 and 0.7 or less, where IA is the intensity of peak A and IB is the intensity of peak B. It is also preferable that the sulfide solid electrolyte has peak C at 2θ=22.0°±0.5° in the X-ray diffraction pattern obtained by performing X-ray diffraction measurement using CuKα1 radiation.