Flat Steel and Method for Producing Same
A flat steel product consisting of (in wt %) 0.1-0.5% C, 1.0-3.0% Mn, 0.9-1.5% Si, ≤1.5% Al, ≤0.008% N, ≤0.020% P, ≤0.005% S, 0.01-1% Cr and optionally one or more of: ≤0.2% Mo, ≤0.01% B, ≤0.5% Cu, ≤0.5% Ni and optionally a total of 0.005-0.2% microalloying elements, the remainder iron and unavoidab...
Gespeichert in:
Hauptverfasser: | , , , , , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | A flat steel product consisting of (in wt %) 0.1-0.5% C, 1.0-3.0% Mn, 0.9-1.5% Si, ≤1.5% Al, ≤0.008% N, ≤0.020% P, ≤0.005% S, 0.01-1% Cr and optionally one or more of: ≤0.2% Mo, ≤0.01% B, ≤0.5% Cu, ≤0.5% Ni and optionally a total of 0.005-0.2% microalloying elements, the remainder iron and unavoidable impurities. The steel has a structure consisting of ≥80 area % martensite, where ≥75 area % is tempered and ≤25 area % is non-tempered, ≥5 volume % residual austenite, 0.5-10 area % ferrite, ≤5 area % bainite, and carbides with a length of ≤250 nm, wherein in the phase boundary between tempered martensite and residual austenite, there is a low-Mn ferrite seam having a width of 4·12 nm and a Mn content of ≤50% of the average Mn content. Also, a method for producing the flat steel in which the structural characteristics of the flat steel product are set by suitable heat treatment. |
---|