LARGE AREA SCINTILLATOR PANELS WITH DOPING
A method of making a scintillator material includes forming a dried ceramic composition into a ceramic body with a garnet crystal formula (Gd3-x-zYx)Cez(Ga5-yAly)O12, where x is about 0 to about 2, y is about 0 to about 5, and z is about 0.001 to about 1.0. The ceramic body is sintered to form a sin...
Gespeichert in:
Hauptverfasser: | , , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | A method of making a scintillator material includes forming a dried ceramic composition into a ceramic body with a garnet crystal formula (Gd3-x-zYx)Cez(Ga5-yAly)O12, where x is about 0 to about 2, y is about 0 to about 5, and z is about 0.001 to about 1.0. The ceramic body is sintered to form a sintered ceramic body. The sintered ceramic body is surrounded by a powder mixture that includes a garnet powder. The density of the sintered ceramic body is increased by applying an increased temperature and isostatic pressure to form the scintillator material. |
---|