METHOD OF TUNING THE CONVERSION TEMPERATURE OF CUBIC PHASE OF ALUMINUM-DOPED LITHIUM LANTHANUM ZIRCONIUM OXIDE
A process for forming cubic LLZO through the use of atomic mixing of metal salts used in an aerosol process. The cubic LLZO is formed at temperatures below 1000° C.