OPTICAL GLASS, PREFORM, AND OPTICAL ELEMENT
The optical glass contains, on a mass % basis, 20.0% to 40.0% of a P2O5 component, 25.0% to 50.0% of a Nb2O5 component, and 3.0% to 30.0% of a total mass (Na2O+K2O), wherein a temperature coefficient (40° C. to 60° C.) of a relative refractive index (589.29 nm) is in the range of +3.0×10−6 to −10.0×...
Gespeichert in:
1. Verfasser: | |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | The optical glass contains, on a mass % basis, 20.0% to 40.0% of a P2O5 component, 25.0% to 50.0% of a Nb2O5 component, and 3.0% to 30.0% of a total mass (Na2O+K2O), wherein a temperature coefficient (40° C. to 60° C.) of a relative refractive index (589.29 nm) is in the range of +3.0×10−6 to −10.0×10−6 (° C.−1). |
---|