COPOLYESTERS PLASTICIZED WITH POLYMERIC PLASTICIZER FOR SHRINK FILM APPLICATIONS

Disclosed is a shrink film containing a copolyester having a minimum crystallization half-time of at least 8.6 minutes and a polyester plasticizer having a weight-average molecular weight of 900 to 12,000 g/mol. The polyester plasticizer includes (i) a polyol component comprising residues of a polyo...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: Shih, Wayne Ken, Kinkade, Nancy Ellen, Carico, Kimberley Carmenia
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Disclosed is a shrink film containing a copolyester having a minimum crystallization half-time of at least 8.6 minutes and a polyester plasticizer having a weight-average molecular weight of 900 to 12,000 g/mol. The polyester plasticizer includes (i) a polyol component comprising residues of a polyol having 2 to 8 carbon atoms, and (ii) a diacid component comprising residues of a dicarboxylic acid having 4 to 12 carbon atoms.