POLYAMIDE FIBER CAPABLE OF HIGH-TEMPERATURE DYEING
The present invention relates to a polyamide fiber which has a single fiber fineness of less than 5 dtex, and has a stress per unit fineness of 0.7 cN/dtex or more in 3% elongation in a tensile test of the fiber, in which a stress F1 in 3% elongation in a tensile test of the fiber before 100°C boili...
Gespeichert in:
Hauptverfasser: | , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | The present invention relates to a polyamide fiber which has a single fiber fineness of less than 5 dtex, and has a stress per unit fineness of 0.7 cN/dtex or more in 3% elongation in a tensile test of the fiber, in which a stress F1 in 3% elongation in a tensile test of the fiber before 100°C boiling water treatment and a stress F2 in 3% elongation in a tensile test of the fiber after the treatment satisfy the following formula (1): F 2 / F 1 > 0.7 |
---|