METHOD TO IMPROVE OPTICAL PROPERTIES OF STABILIZED POLYCARBONATE COMPOSITIONS
Methods for producing transparent polycarbonate articles include melting a composition at a temperature of 300 to 390° C., extruding the melted composition to form a strand, cooling the strand of extruded composition, cutting the cooled strand into pellets, drying the pellets at a temperature of 50...
Gespeichert in:
Hauptverfasser: | , , , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | Methods for producing transparent polycarbonate articles include melting a composition at a temperature of 300 to 390° C., extruding the melted composition to form a strand, cooling the strand of extruded composition, cutting the cooled strand into pellets, drying the pellets at a temperature of 50 to 140° C. and injecting molding or extruding the pellets at a temperature of 300 to 380° C. to form an article. The composition can comprise a moisture content of 0.1 to 5 wt. % and a crystalline additive having a melting point of at least 280° C., a heat of fusion greater than or equal to 1.0 Joule/gram (J/g). The composition can be cooled to at least 20° C. below the glass transition temperature of the polycarbonate. |
---|