METHOD OF MANUFACTURING SEMICONDUCTOR DEVICE
An impurity of a second conductivity type is selectively doped in a surface of a semiconductor substrate of a first conductivity type to form doped regions. A portion of a surface of the doped regions is covered by a heat insulating film. At least a remaining portion of the surface of the doped regi...
Gespeichert in:
Hauptverfasser: | , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | An impurity of a second conductivity type is selectively doped in a surface of a semiconductor substrate of a first conductivity type to form doped regions. A portion of a surface of the doped regions is covered by a heat insulating film. At least a remaining portion of the surface of the doped regions is covered by an absorbing film and the doped regions are heated through the absorbing film, enabling an impurity region of the second conductivity type to be formed having two or more of the doped regions that have a same impurity concentration and differing carrier concentrations. |
---|