BONDED ABRASIVE ARTICLE AND METHOD OF GRINDING
An abrasive article configured to grind a workpiece having a fracture toughness of at least about 5.5 MPa·m0.5 may include a body comprising abrasive particles contained within a bond material comprising a metal, wherein the body comprises a ratio of VAG/VBM of at least about 1.3, wherein VAG is a v...
Gespeichert in:
Hauptverfasser: | , , , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | Lane, William H Ramanath, Srinivasan Hitchiner, Michael P Upadhyay, Rachana |
description | An abrasive article configured to grind a workpiece having a fracture toughness of at least about 5.5 MPa·m0.5 may include a body comprising abrasive particles contained within a bond material comprising a metal, wherein the body comprises a ratio of VAG/VBM of at least about 1.3, wherein VAG is a volume percent of abrasive particles within a total volume of the body and VBM is a volume percent of bond material within the total volume of the body, and wherein the abrasive particles have an average particle size of at least about 1 micron and not greater than about 20 microns. |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_US2018117736A1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>US2018117736A1</sourcerecordid><originalsourceid>FETCH-epo_espacenet_US2018117736A13</originalsourceid><addsrcrecordid>eNrjZNBz8vdzcXVRcHQKcgz2DHNVcAwK8XT2AdJ-Lgq-riEe_i4K_m4K7kGefi6efu48DKxpiTnFqbxQmptB2c01xNlDN7UgPz61uCAxOTUvtSQ-NNjIwNDC0NDc3NjM0dCYOFUASkwmSQ</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>BONDED ABRASIVE ARTICLE AND METHOD OF GRINDING</title><source>esp@cenet</source><creator>Lane, William H ; Ramanath, Srinivasan ; Hitchiner, Michael P ; Upadhyay, Rachana</creator><creatorcontrib>Lane, William H ; Ramanath, Srinivasan ; Hitchiner, Michael P ; Upadhyay, Rachana</creatorcontrib><description>An abrasive article configured to grind a workpiece having a fracture toughness of at least about 5.5 MPa·m0.5 may include a body comprising abrasive particles contained within a bond material comprising a metal, wherein the body comprises a ratio of VAG/VBM of at least about 1.3, wherein VAG is a volume percent of abrasive particles within a total volume of the body and VBM is a volume percent of bond material within the total volume of the body, and wherein the abrasive particles have an average particle size of at least about 1 micron and not greater than about 20 microns.</description><language>eng</language><subject>GRINDING ; PERFORMING OPERATIONS ; POLISHING ; TOOLS FOR GRINDING, BUFFING, OR SHARPENING ; TRANSPORTING</subject><creationdate>2018</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20180503&DB=EPODOC&CC=US&NR=2018117736A1$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20180503&DB=EPODOC&CC=US&NR=2018117736A1$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>Lane, William H</creatorcontrib><creatorcontrib>Ramanath, Srinivasan</creatorcontrib><creatorcontrib>Hitchiner, Michael P</creatorcontrib><creatorcontrib>Upadhyay, Rachana</creatorcontrib><title>BONDED ABRASIVE ARTICLE AND METHOD OF GRINDING</title><description>An abrasive article configured to grind a workpiece having a fracture toughness of at least about 5.5 MPa·m0.5 may include a body comprising abrasive particles contained within a bond material comprising a metal, wherein the body comprises a ratio of VAG/VBM of at least about 1.3, wherein VAG is a volume percent of abrasive particles within a total volume of the body and VBM is a volume percent of bond material within the total volume of the body, and wherein the abrasive particles have an average particle size of at least about 1 micron and not greater than about 20 microns.</description><subject>GRINDING</subject><subject>PERFORMING OPERATIONS</subject><subject>POLISHING</subject><subject>TOOLS FOR GRINDING, BUFFING, OR SHARPENING</subject><subject>TRANSPORTING</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2018</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZNBz8vdzcXVRcHQKcgz2DHNVcAwK8XT2AdJ-Lgq-riEe_i4K_m4K7kGefi6efu48DKxpiTnFqbxQmptB2c01xNlDN7UgPz61uCAxOTUvtSQ-NNjIwNDC0NDc3NjM0dCYOFUASkwmSQ</recordid><startdate>20180503</startdate><enddate>20180503</enddate><creator>Lane, William H</creator><creator>Ramanath, Srinivasan</creator><creator>Hitchiner, Michael P</creator><creator>Upadhyay, Rachana</creator><scope>EVB</scope></search><sort><creationdate>20180503</creationdate><title>BONDED ABRASIVE ARTICLE AND METHOD OF GRINDING</title><author>Lane, William H ; Ramanath, Srinivasan ; Hitchiner, Michael P ; Upadhyay, Rachana</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_US2018117736A13</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2018</creationdate><topic>GRINDING</topic><topic>PERFORMING OPERATIONS</topic><topic>POLISHING</topic><topic>TOOLS FOR GRINDING, BUFFING, OR SHARPENING</topic><topic>TRANSPORTING</topic><toplevel>online_resources</toplevel><creatorcontrib>Lane, William H</creatorcontrib><creatorcontrib>Ramanath, Srinivasan</creatorcontrib><creatorcontrib>Hitchiner, Michael P</creatorcontrib><creatorcontrib>Upadhyay, Rachana</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>Lane, William H</au><au>Ramanath, Srinivasan</au><au>Hitchiner, Michael P</au><au>Upadhyay, Rachana</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>BONDED ABRASIVE ARTICLE AND METHOD OF GRINDING</title><date>2018-05-03</date><risdate>2018</risdate><abstract>An abrasive article configured to grind a workpiece having a fracture toughness of at least about 5.5 MPa·m0.5 may include a body comprising abrasive particles contained within a bond material comprising a metal, wherein the body comprises a ratio of VAG/VBM of at least about 1.3, wherein VAG is a volume percent of abrasive particles within a total volume of the body and VBM is a volume percent of bond material within the total volume of the body, and wherein the abrasive particles have an average particle size of at least about 1 micron and not greater than about 20 microns.</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | eng |
recordid | cdi_epo_espacenet_US2018117736A1 |
source | esp@cenet |
subjects | GRINDING PERFORMING OPERATIONS POLISHING TOOLS FOR GRINDING, BUFFING, OR SHARPENING TRANSPORTING |
title | BONDED ABRASIVE ARTICLE AND METHOD OF GRINDING |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-20T02%3A25%3A43IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=Lane,%20William%20H&rft.date=2018-05-03&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EUS2018117736A1%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |