GLASS COMPOSITION, GLASS COMPOSITION FOR CHEMCIAL STRENGTHENING, STRENGTHENED GLASS ARTICLE, AND COVER GLASS FOR DISPLAY
A glass composition of the present invention includes, in mol %, 66 to 72% SiO2, 1 to 4% Al2O3, 8 to 15% MgO, 1 to 8% CaO, 12 to 16% Na2O, and 0 to 1% K2O. A total content of MgO and CaO is in a range of 12 to 17%, and a molar ratio of CaO to the total content of MgO and CaO is in a range of 0.1 to...
Gespeichert in:
Hauptverfasser: | , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | A glass composition of the present invention includes, in mol %, 66 to 72% SiO2, 1 to 4% Al2O3, 8 to 15% MgO, 1 to 8% CaO, 12 to 16% Na2O, and 0 to 1% K2O. A total content of MgO and CaO is in a range of 12 to 17%, and a molar ratio of CaO to the total content of MgO and CaO is in a range of 0.1 to 0.4. The glass composition of the present invention is suitable for production by the float process, and is suitable for chemical strengthening. |
---|