NICKEL COMPOSITE HYDROXIDE PARTICLES AND NONAQUEOUS ELECTROLYTE SECONDARY BATTERY
To provide nickel composite hydroxide particles having a small and uniform particle diameter and a method for producing the same. The method for producing the nickel composite hydroxide particles includes: a nucleation step of producing nuclei including primary particles by controlling a pH of an aq...
Gespeichert in:
Hauptverfasser: | , , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | To provide nickel composite hydroxide particles having a small and uniform particle diameter and a method for producing the same. The method for producing the nickel composite hydroxide particles includes: a nucleation step of producing nuclei including primary particles by controlling a pH of an aqueous solution for nucleation to 11.5 to 13.2 at a liquid temperature of 25° C., the aqueous solution for nucleation containing a metal compound having an atomic ratio of metals corresponding to an atomic ratio of metals in the nickel composite hydroxide particles and substantially not containing a metal complex ion-forming agent; and a particle growth step of forming, on an outer surface of each of the nuclei, an outer shell portion including platy primary particles larger than primary particles of the nuclei by controlling a pH of an aqueous solution for particle growth containing the nuclei obtained in the nucleation step to 9.5 to 11.0 at a liquid temperature of 25° C. |
---|