METHOD FOR PRODUCING CHROMIUM (III) OXIDE
Process for preparing chromium(III) oxide, comprising the steps of: a) Decomposing an alkali metal ammonium chromate double salt at a temperature of 200 to 650° C., especially of 250 to 550° C., b) washing the decomposition product obtained after a) and c) calcining the product obtained after b) at...
Gespeichert in:
Hauptverfasser: | , , , , , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | Process for preparing chromium(III) oxide, comprising the steps of: a) Decomposing an alkali metal ammonium chromate double salt at a temperature of 200 to 650° C., especially of 250 to 550° C., b) washing the decomposition product obtained after a) and c) calcining the product obtained after b) at a temperature of 700 to 1400° C., especially of 800 to 1300° C. |
---|