Precious metal catalysts with low metal loading for oxidative dehydrogenations

A method of production of a catalyst that has 0.05-0.25 wt. % of precious metal, preferably for the oxidative dehydrogenation of olefinically unsaturated alcohols, comprising the following steps a) producing a D.C. plasma, b) introducing the metal and support material into the plasma, c) evaporating...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: MAEURER TORSTEN, BALTES CHRISTIAN, GROSSSCHMIDT DIRK, SEEBER GEORG
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:A method of production of a catalyst that has 0.05-0.25 wt. % of precious metal, preferably for the oxidative dehydrogenation of olefinically unsaturated alcohols, comprising the following steps a) producing a D.C. plasma, b) introducing the metal and support material into the plasma, c) evaporating the metal and support material or shattering the solid bodies of metal and support material in the plasma, and reaction of the particles, d) cooling, so that very small particles of composite material are obtained, e) applying the composite material on the catalyst support proper, the correspondingly produced catalyst and use thereof.