Stable, concentratable, water soluble cellulose free chemical mechanical polishing composition
A chemical mechanical polishing composition useful for chemical mechanical polishing a semiconductor wafer containing an interconnect metal is provided, comprising, as initial components: water; an azole inhibitor; an alkali metal organic surfactant; a hydrotrope; a phosphorus containing agent; opti...
Gespeichert in:
Hauptverfasser: | , , , , , , , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | A chemical mechanical polishing composition useful for chemical mechanical polishing a semiconductor wafer containing an interconnect metal is provided, comprising, as initial components: water; an azole inhibitor; an alkali metal organic surfactant; a hydrotrope; a phosphorus containing agent; optionally, a non-saccharide water soluble polymer; optionally, a water soluble acid compound of formula I, wherein R is selected from a hydrogen and a C1-5 alkyl group, and wherein x is 1 or 2; optionally, a complexing agent; optionally, an oxidizer; optionally, an organic solvent; and, optionally, an abrasive. Also, provided is a method for making a chemical mechanical polishing composition of the present invention and a method for chemical mechanical polishing of a substrate, comprising: providing a substrate, wherein the substrate is a semiconductor wafer having copper interconnects; providing a chemical mechanical polishing composition of the present invention; providing a chemical mechanical polishing pad; creating dynamic contact at an interface between the chemical mechanical polishing pad and the substrate with a down force of 0.69 to 34.5 kPa; and, dispensing the chemical mechanical polishing composition onto the chemical mechanical polishing pad at or near the interface between the chemical mechanical polishing pad and the substrate; wherein the chemical mechanical polishing composition exhibits a pH adjusted to a pH of 2 to 6 through the addition of at least one of phosphoric acid, magnesium hydroxide and lithium hydroxide. |
---|