LOW TEMPERATURE CURABLE AMORPHOUS FLUOROPOLYMERS

There is provided a comprising an amorphous peroxide curable fluoropolymer comprising an iodine, bromine or chlorine containing cure site, an organic peroxide with a 10-hour half life temperature below 90° C., and a coagent, where the amorphous fluoropolymer has a storage modulus at 25° C. and 0.1 r...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: FUKUSHI TATSUO, WELLNER STEVEN J
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:There is provided a comprising an amorphous peroxide curable fluoropolymer comprising an iodine, bromine or chlorine containing cure site, an organic peroxide with a 10-hour half life temperature below 90° C., and a coagent, where the amorphous fluoropolymer has a storage modulus at 25° C. and 0.1 rad/s of less than or equal to 300 kPa, and also where the fluropolymer 90% cure time as measured by sealed torsion shear rotorless curemeter in ASTM D5289-07 is less than 30 minutes at 110° C. There is also provided a fluoroelastomer preparable by curing such composition. There is further provided a cure in place process using such composition to create a cure in place article and cure in place articles from such process.