Alternate pad structures/passivation inegration schemes to reduce or eliminate IMC cracking in post wire bonded dies during Cu/Low-K BEOL processing

Passivation integration schemes and pad structures to reduce the stress gradients and/or improve the contact surface existing between the Al in the pad and the gold wire bond. One of the pad structures provides a plurality of recessed pad areas which are formed in a single aluminum pad. An oxide mes...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: PALLINTI JAYANTHI, SUN SEY-SHING, BHATT HEMANSHU, KAO CHIYI, YING HONG, VIJAY DILIP
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator PALLINTI JAYANTHI
SUN SEY-SHING
BHATT HEMANSHU
KAO CHIYI
YING HONG
VIJAY DILIP
description Passivation integration schemes and pad structures to reduce the stress gradients and/or improve the contact surface existing between the Al in the pad and the gold wire bond. One of the pad structures provides a plurality of recessed pad areas which are formed in a single aluminum pad. An oxide mesa can be provided under the aluminum pad. Another pad structure provides a single recessed pad area which is formed in a single aluminum pad, and the aluminum pad is disposed above a copper pad and a plurality of trench/via pads. Still another pad structure provides a single recessed pad area which is formed in a single aluminum pad, and the aluminum pad is disposed above a portion of a copper pad, such that the aluminum pad and the copper pad are staggered relative to each other.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_US2007114667A1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>US2007114667A1</sourcerecordid><originalsourceid>FETCH-epo_espacenet_US2007114667A13</originalsourceid><addsrcrecordid>eNqNjUFuwjAURLNhUQF3-FLXUQhUYQ1RqlalYkG7jow9DRaJbf1vw0U4cEPbA3Q1I828mYfstukj2KkICsqQRE46JoYUQYnYi4rWO7IOHf9a0ScMEIqeGCZpkGdCbwf7M_L6XpNmpc_WdSNGwUukq2XQ0TsDQ8aOsEl8z-tU7Pw1f6Nts99RYK8xfrpulk2-VC-Y_-k0e3xuPuqXHMG3kKA0HGL7eVguFuuyfKqq9aZc_a_1DRU7UPE</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Alternate pad structures/passivation inegration schemes to reduce or eliminate IMC cracking in post wire bonded dies during Cu/Low-K BEOL processing</title><source>esp@cenet</source><creator>PALLINTI JAYANTHI ; SUN SEY-SHING ; BHATT HEMANSHU ; KAO CHIYI ; YING HONG ; VIJAY DILIP</creator><creatorcontrib>PALLINTI JAYANTHI ; SUN SEY-SHING ; BHATT HEMANSHU ; KAO CHIYI ; YING HONG ; VIJAY DILIP</creatorcontrib><description>Passivation integration schemes and pad structures to reduce the stress gradients and/or improve the contact surface existing between the Al in the pad and the gold wire bond. One of the pad structures provides a plurality of recessed pad areas which are formed in a single aluminum pad. An oxide mesa can be provided under the aluminum pad. Another pad structure provides a single recessed pad area which is formed in a single aluminum pad, and the aluminum pad is disposed above a copper pad and a plurality of trench/via pads. Still another pad structure provides a single recessed pad area which is formed in a single aluminum pad, and the aluminum pad is disposed above a portion of a copper pad, such that the aluminum pad and the copper pad are staggered relative to each other.</description><language>eng</language><subject>BASIC ELECTRIC ELEMENTS ; ELECTRIC SOLID STATE DEVICES NOT OTHERWISE PROVIDED FOR ; ELECTRICITY ; SEMICONDUCTOR DEVICES</subject><creationdate>2007</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20070524&amp;DB=EPODOC&amp;CC=US&amp;NR=2007114667A1$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76289</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20070524&amp;DB=EPODOC&amp;CC=US&amp;NR=2007114667A1$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>PALLINTI JAYANTHI</creatorcontrib><creatorcontrib>SUN SEY-SHING</creatorcontrib><creatorcontrib>BHATT HEMANSHU</creatorcontrib><creatorcontrib>KAO CHIYI</creatorcontrib><creatorcontrib>YING HONG</creatorcontrib><creatorcontrib>VIJAY DILIP</creatorcontrib><title>Alternate pad structures/passivation inegration schemes to reduce or eliminate IMC cracking in post wire bonded dies during Cu/Low-K BEOL processing</title><description>Passivation integration schemes and pad structures to reduce the stress gradients and/or improve the contact surface existing between the Al in the pad and the gold wire bond. One of the pad structures provides a plurality of recessed pad areas which are formed in a single aluminum pad. An oxide mesa can be provided under the aluminum pad. Another pad structure provides a single recessed pad area which is formed in a single aluminum pad, and the aluminum pad is disposed above a copper pad and a plurality of trench/via pads. Still another pad structure provides a single recessed pad area which is formed in a single aluminum pad, and the aluminum pad is disposed above a portion of a copper pad, such that the aluminum pad and the copper pad are staggered relative to each other.</description><subject>BASIC ELECTRIC ELEMENTS</subject><subject>ELECTRIC SOLID STATE DEVICES NOT OTHERWISE PROVIDED FOR</subject><subject>ELECTRICITY</subject><subject>SEMICONDUCTOR DEVICES</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2007</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNjUFuwjAURLNhUQF3-FLXUQhUYQ1RqlalYkG7jow9DRaJbf1vw0U4cEPbA3Q1I828mYfstukj2KkICsqQRE46JoYUQYnYi4rWO7IOHf9a0ScMEIqeGCZpkGdCbwf7M_L6XpNmpc_WdSNGwUukq2XQ0TsDQ8aOsEl8z-tU7Pw1f6Nts99RYK8xfrpulk2-VC-Y_-k0e3xuPuqXHMG3kKA0HGL7eVguFuuyfKqq9aZc_a_1DRU7UPE</recordid><startdate>20070524</startdate><enddate>20070524</enddate><creator>PALLINTI JAYANTHI</creator><creator>SUN SEY-SHING</creator><creator>BHATT HEMANSHU</creator><creator>KAO CHIYI</creator><creator>YING HONG</creator><creator>VIJAY DILIP</creator><scope>EVB</scope></search><sort><creationdate>20070524</creationdate><title>Alternate pad structures/passivation inegration schemes to reduce or eliminate IMC cracking in post wire bonded dies during Cu/Low-K BEOL processing</title><author>PALLINTI JAYANTHI ; SUN SEY-SHING ; BHATT HEMANSHU ; KAO CHIYI ; YING HONG ; VIJAY DILIP</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_US2007114667A13</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2007</creationdate><topic>BASIC ELECTRIC ELEMENTS</topic><topic>ELECTRIC SOLID STATE DEVICES NOT OTHERWISE PROVIDED FOR</topic><topic>ELECTRICITY</topic><topic>SEMICONDUCTOR DEVICES</topic><toplevel>online_resources</toplevel><creatorcontrib>PALLINTI JAYANTHI</creatorcontrib><creatorcontrib>SUN SEY-SHING</creatorcontrib><creatorcontrib>BHATT HEMANSHU</creatorcontrib><creatorcontrib>KAO CHIYI</creatorcontrib><creatorcontrib>YING HONG</creatorcontrib><creatorcontrib>VIJAY DILIP</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>PALLINTI JAYANTHI</au><au>SUN SEY-SHING</au><au>BHATT HEMANSHU</au><au>KAO CHIYI</au><au>YING HONG</au><au>VIJAY DILIP</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Alternate pad structures/passivation inegration schemes to reduce or eliminate IMC cracking in post wire bonded dies during Cu/Low-K BEOL processing</title><date>2007-05-24</date><risdate>2007</risdate><abstract>Passivation integration schemes and pad structures to reduce the stress gradients and/or improve the contact surface existing between the Al in the pad and the gold wire bond. One of the pad structures provides a plurality of recessed pad areas which are formed in a single aluminum pad. An oxide mesa can be provided under the aluminum pad. Another pad structure provides a single recessed pad area which is formed in a single aluminum pad, and the aluminum pad is disposed above a copper pad and a plurality of trench/via pads. Still another pad structure provides a single recessed pad area which is formed in a single aluminum pad, and the aluminum pad is disposed above a portion of a copper pad, such that the aluminum pad and the copper pad are staggered relative to each other.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_US2007114667A1
source esp@cenet
subjects BASIC ELECTRIC ELEMENTS
ELECTRIC SOLID STATE DEVICES NOT OTHERWISE PROVIDED FOR
ELECTRICITY
SEMICONDUCTOR DEVICES
title Alternate pad structures/passivation inegration schemes to reduce or eliminate IMC cracking in post wire bonded dies during Cu/Low-K BEOL processing
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-08T17%3A30%3A57IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=PALLINTI%20JAYANTHI&rft.date=2007-05-24&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EUS2007114667A1%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true