The present invention relates to a cemented carbide body containing from about 3 to less than about 15 wt-% binder phase and essentially WC as the remainder. By alloying the binder phase with from about 0.5 to about 15 wt-% Mn an increase in the strength of the WC/WC grain boundaries is obtained.

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: NORGREN SUSANNE, CHRISTENSEN MIKAEL, WAHNSTROM GORAN
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:The present invention relates to a cemented carbide body containing from about 3 to less than about 15 wt-% binder phase and essentially WC as the remainder. By alloying the binder phase with from about 0.5 to about 15 wt-% Mn an increase in the strength of the WC/WC grain boundaries is obtained.