Method of preparing silicas, silicas with specific pore-size and/or particle-size distribution, and the uses thereof, in particular for reinforcing polymers
The invention relates to a novel method of preparing silicas and to highly-structured silicas having the following characteristics: a specific surface area CTAB (SCTAB) of between 40 and 525 m2/g; a specific surface area BET (SBET) of between 45 and 550 m2/g; an object size distribution width Ld ((d...
Gespeichert in:
1. Verfasser: | |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | The invention relates to a novel method of preparing silicas and to highly-structured silicas having the following characteristics: a specific surface area CTAB (SCTAB) of between 40 and 525 m2/g; a specific surface area BET (SBET) of between 45 and 550 m2/g; an object size distribution width Ld ((d84-d16)/d50), which is measured by XDC particle size analysis after deagglomeration with ultrasound, of at least 0.91; and a pore-size distribution such that ratio V(d5-d50)/V(d5-d100) is at least 0.66. The invention also relates to the use of said silicas as polymer reinforcing fillers. |
---|