Thermoplastic resin compositon and its injection molded article
Disclosed is a thermoplastic resin composition comprising (A) 35 to 85% by weight of a polypropylene resin, (B) 10 to 35% by weight of an elastomer, (C) 2 to 30% by weight of an inorganic filler and (D) 5 to 15% by weight of a resin, wherein the resin (D) has a melt tension (MT), measured at a windi...
Gespeichert in:
Hauptverfasser: | , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | Disclosed is a thermoplastic resin composition comprising (A) 35 to 85% by weight of a polypropylene resin, (B) 10 to 35% by weight of an elastomer, (C) 2 to 30% by weight of an inorganic filler and (D) 5 to 15% by weight of a resin, wherein the resin (D) has a melt tension (MT), measured at a winding speed of 15.7 m/min, of not less than 0.03 N and less than 0.1 N and a swelling ratio (SR), measured at 220° C., an L/D of an orifice of 40 and a shear rate of 1.2x103 sec-1, of 1.8 or more, and the time required for the resin (D) until the ratio (G(t)/G(0.02)) of the relaxation elastic modulus G(t) measured at 210° C. to the relaxation elastic modulus G(0.02) in a time of 0.02 second reaches 0.01 is not less than 5 seconds and less than 10 seconds. |
---|