Method for producing Ti-Ai alloy
Production methods for Ti-Al alloys may include: adding a flux including calcium oxide containing 35+wt. % calcium fluoride, to a melt starting material of Ti material and Al material and with 50+wt. % Al; introducing the fluxed melt starting material into a water-cooled copper crucible having a tap...
Gespeichert in:
Hauptverfasser: | , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | Production methods for Ti-Al alloys may include: adding a flux including calcium oxide containing 35+wt. % calcium fluoride, to a melt starting material of Ti material and Al material and with 50+wt. % Al; introducing the fluxed melt starting material into a water-cooled copper crucible having a tapping port in the bottom, induction melting it inside the water-cooled copper crucible in at least a 1.33 Pa atmosphere; the flux, containing oxygen released from the melt starting material by the induction melting, is separated out by tapping the melt starting material, which was induction melted in the water-cooled copper crucible, downward from the tapping port; and when obtaining the Ti-Al alloy by casting the flux-removed melt starting material, the induction melting output is reduced to no more than 90% of that during melting and tapping is performed from the water-cooled crucible with the output in a reduced state. |
---|