Semi-aromatic polyamide fiber and method for producing same

Provided is a semi-aromatic polyamide fiber having excellent spinning stability, heat resistance and chemical resistance. The semi-aromatic polyamide fiber includes a semi-aromatic polyamide resin having a melting point of 290° C. or higher and a plasticizer having a 5% thermal weight reduction temp...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: Washitake, Yosuke, Tsudaka, Takeshi, Tsunofuri, Shohei
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Provided is a semi-aromatic polyamide fiber having excellent spinning stability, heat resistance and chemical resistance. The semi-aromatic polyamide fiber includes a semi-aromatic polyamide resin having a melting point of 290° C. or higher and a plasticizer having a 5% thermal weight reduction temperature of 320° C. or higher, the resin having as a dicarboxylic acid component an aromatic dicarboxylic acid unit and as a diamine component 1,9-nonanediamine unit and 2-methyl-1,8-octanediamine unit in a molar ratio (the former:the latter) of 70:30 to 99:1.