Superalloy with optimized properties and a limited density
A nickel-based superalloy includes, in atomic percentages, 13% to 21% chromium, 15% to 26% cobalt, 4% to 8% aluminum, 4.5% to 8% titanium, 8% to 18% iron, boron in an atomic percentage less than or equal to 0.5% or no boron, carbon in an atomic percentage less than or equal to 1% or no carbon, at le...
Gespeichert in:
Hauptverfasser: | , , , , , , , , , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | A nickel-based superalloy includes, in atomic percentages, 13% to 21% chromium, 15% to 26% cobalt, 4% to 8% aluminum, 4.5% to 8% titanium, 8% to 18% iron, boron in an atomic percentage less than or equal to 0.5% or no boron, carbon in an atomic percentage less than or equal to 1% or no carbon, at least one additional element selected from molybdenum, tungsten, tantalum and niobium, a total atomic content of the at least one additional element being less than or equal to 1.5% or no such at least one additional element, the remainder being nickel and unavoidable impurities, with a sum of the atomic percentages of aluminum and titanium being comprised between 8.5% and 15%. The novel superalloy composition has a limited density and exhibiting, when hot, good mechanical properties as well as good resistance to oxidation and corrosion. |
---|