Preparation method of improved sintered neodymium-iron-boron (Nd-Fe-B) casting strip

A preparation method of improved sintered neodymium-iron-boron (Nd-Fe-B) casting strips includes the following steps: firstly nucleation assisted alloy particles used for sintered Nd-Fe-B casting strips are prepared, all elements are weighted as follows: 26.68-28% of Pr-Nd, 70-72.5% of Fe and 0.90-1...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: Liu, Jixiang, Xia, Feng, Sun, Caina, Gao, Jiao, Feng, Yonghuai, Li, Yanli, Wang, Yu
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:A preparation method of improved sintered neodymium-iron-boron (Nd-Fe-B) casting strips includes the following steps: firstly nucleation assisted alloy particles used for sintered Nd-Fe-B casting strips are prepared, all elements are weighted as follows: 26.68-28% of Pr-Nd, 70-72.5% of Fe and 0.90-1% of B, and a Pr element in two elements of Pr-Nd accounts for 0-30 wt %; the compounded materials are smelted and poured to obtain alloy strips, then the alloy strips are crushed into particles with diameter of 1-10 mm; secondly, Nd-Fe-B casting strips are prepared: the prepared intermediate materials are smelted and melted into molten steel, and then are refined; after the intermediate materials are fully melted, the nucleation assisted alloy particles are added; and after the nucleation assisted alloy particles are added, smelting is performed for 3-15 minutes pouring is performed, and final Nd-Fe-B alloy casting strips are obtained.