Process for preparing metal-chelate retarder by sol-gel method

The present invention relates to a process for preparing a metal-chelate retarder by a sol-gel method. The method comprises the following steps: weighing calcium nitrate tetrahydrate, aluminum nitrate nonahydrate and ferric nitrate nonahydrate according to a certain mass ratio and adding them into d...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: Wu, Chaoming, Liu, Wenming, Lin, Zhihui, Fu, Jiawen, Liu, Kaiqiang, Li, Zaoyuan, Huang, Sheng, Zhang, Chunmei, Guo, Xiaoyang, Yu, Yang, Qi, Ben, Zhang, Gaoyin, Cheng, Xiaowei, Zuo, Tianpeng, Zhao, Shuxun, Chen, Zuwei
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:The present invention relates to a process for preparing a metal-chelate retarder by a sol-gel method. The method comprises the following steps: weighing calcium nitrate tetrahydrate, aluminum nitrate nonahydrate and ferric nitrate nonahydrate according to a certain mass ratio and adding them into deionized water; placing the mixed solution on a magnetic stirrer and stirring the mixed solution evenly; adding citric acid monohydrate or gluconic acid, ethylene glycol or glycerol, and placing the mixed solution into a water bath to react to obtain the metal-chelate retarder. The process of the present invention has a reliable principle, overcomes the defects of long production period, complex preparation and the like of the existing retarders, has the advantages of simple process operation, cheap and easily available raw materials, and short production period. The prepared retarder has wide temperature adaptation range and adjustable thickening time, is suitable for large-scale industrial production, and has a wide market application prospect.