Methods for chromium catalyst activation using oxygen-enriched fluidization gas
Processes for producing an activated chromium catalyst are disclosed, and these processes comprise contacting a supported chromium catalyst with a gas stream containing from 25-60 vol % oxygen at a peak activation temperature of 550-900° C. to produce the activated chromium catalyst. The linear velo...
Gespeichert in:
Hauptverfasser: | , , , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | Processes for producing an activated chromium catalyst are disclosed, and these processes comprise contacting a supported chromium catalyst with a gas stream containing from 25-60 vol % oxygen at a peak activation temperature of 550-900° C. to produce the activated chromium catalyst. The linear velocity of the gas stream is 0.18-0.4 ft/sec, and the oxygen linear velocity of the gas stream is 0.05-0.15 ft/sec. The resultant activated chromium catalyst and an optional co-catalyst can be contacted with an olefin monomer and an optional olefin comonomer in a polymerization reactor system under polymerization conditions to produce an olefin polymer. |
---|