Process for making a mixed metal oxide
A process for making a mixed metal oxide, may involve: (a) providing a hydroxide or oxyhydroxide of TM with an average particle diameter (D50) in the range of from 0.1 μm to 5 mm; (b) subjecting the hydroxide or oxyhydroxide of TM to a stream of gas with a temperature in the range of from 150 to 200...
Gespeichert in:
Hauptverfasser: | , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | A process for making a mixed metal oxide, may involve: (a) providing a hydroxide or oxyhydroxide of TM with an average particle diameter (D50) in the range of from 0.1 μm to 5 mm; (b) subjecting the hydroxide or oxyhydroxide of TM to a stream of gas with a temperature in the range of from 150 to 2000° C., wherein TM contains nickel and at least one further transition metal selected from cobalt and manganese. |
---|