Barrier film with enhanced formability and a method for making thereof

A film comprises an outer heat sealable layer mainly made of a (co)polyolefin with the Vicat softening temperature not exceeding 130° C., at least one heat resistant layer mainly made of at least one polar (co)polymer selected from the group including predominantly aliphatic (co)polyamides and aroma...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: Biryukov, Vadim Yurievich, Kostrub, Vladimir Vladimirovich, Verin, Sergey Vladimirovich, Golyanskiy, Boris Vladimirovich, Burykin, Igor Vladimirovich
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:A film comprises an outer heat sealable layer mainly made of a (co)polyolefin with the Vicat softening temperature not exceeding 130° C., at least one heat resistant layer mainly made of at least one polar (co)polymer selected from the group including predominantly aliphatic (co)polyamides and aromatic (co)polyesters, and at least one core adhesive layer from a material capable of adhering both to (co)polyolefins and to polar (co)polymers. The heat resistant layer comprises not less than 15% of at least one predominantly aliphatic copolyamide with the melting temperature not exceeding 205° C. A method comprises the stages of coextrusion, biaxial stretching, annealing and winding up of the resulting film into a roll.