Heat-resistant alloy, and reaction tube
The present invention provides a heat-resistant alloy and a reaction tube having excellent oxidation resistance, excellent mechanical properties such as tensile ductility, and weldability. A heat-resistant alloy of the present invention comprises, in terms of % by mass, C: 0.35% to 0.7%, Si: more th...
Gespeichert in:
Hauptverfasser: | , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | The present invention provides a heat-resistant alloy and a reaction tube having excellent oxidation resistance, excellent mechanical properties such as tensile ductility, and weldability. A heat-resistant alloy of the present invention comprises, in terms of % by mass, C: 0.35% to 0.7%, Si: more than 0% and 1.5% or less, Mn: more than 0% and 2.0% or less, Cr: 22.0% to 40.0%, Ni: 25.0% to 48.3%, Al: 1.5% to 4.5%, Ti: 0.01% to 0.6%, and the balance being Fe and inevitable impurities, wherein when Pa=−11.1+28.1×C+29.2×Si−0.25×Ni−45.6×Ti, and Ya=−13.75×Al+63.75, Pa |
---|