Triblock copolymers
Described is a triblock copolymer of the formula ABC wherein B is a hydrogenated vinyl aromatic block having a Tg of ≥110° C. and comprising 30-90 wt. % of the copolymer; C is a rubbery block having a Tg≤25° C. and comprising 10-70 wt. % of the copolymer; and A is an block derived from ring-opening...
Gespeichert in:
Hauptverfasser: | , , , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | Described is a triblock copolymer of the formula ABC wherein B is a hydrogenated vinyl aromatic block having a Tg of ≥110° C. and comprising 30-90 wt. % of the copolymer; C is a rubbery block having a Tg≤25° C. and comprising 10-70 wt. % of the copolymer; and A is an block derived from ring-opening polymerization, substantially incompatible with both B and C blocks. |
---|