Austenitic steel having excellent machinability and ultra-low temperature toughness in weld heat-affected zone, and method of manufacturing the same
According to the present invention, a low-cost ultra-low temperature steel may be obtained, a stable austenite phase may be formed at low temperature, carbide formation may be effectively suppressed, and a structural steel having excellent machinability and ultra-low temperature toughness in a weld...
Gespeichert in:
Hauptverfasser: | , , , , , , , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | According to the present invention, a low-cost ultra-low temperature steel may be obtained, a stable austenite phase may be formed at low temperature, carbide formation may be effectively suppressed, and a structural steel having excellent machinability and ultra-low temperature toughness in a weld heat-affected zone may be provided. |
---|