Method for determining defect region
A method for determining a defect region of a silicon wafer which is sliced off from a silicon single crystal manufactured by a CZ method, the method including: (1) mirror-surface processing the silicon wafer in such a manner that a haze level of a surface thereof in haze measurement performed by a...
Gespeichert in:
Hauptverfasser: | , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | A method for determining a defect region of a silicon wafer which is sliced off from a silicon single crystal manufactured by a CZ method, the method including: (1) mirror-surface processing the silicon wafer in such a manner that a haze level of a surface thereof in haze measurement performed by a particle counter which uses a laser having a wavelength of 266 nm becomes 0.06 ppm or less; (2) measuring the number of defects and/or a defect density distribution on the mirror-surface-processed surface of the silicon wafer by using a particle counter capable of measuring defects having a size of 15 nm or less; and (3) determining the defect region of the silicon wafer from the measured number of the defects and/or defect density distribution. |
---|