Adhesive composition for polarizing plate
An adhesive composition for a polarizing plate is adapted to exhibit a variation in relaxation modulus of an adhesive layer in a range of 75% to 95% before and after leaving the same at a temperature of −20° C. to 0° C. for 4 hours, such that it is possible to remarkably improve thermal-shock durabi...
Gespeichert in:
Hauptverfasser: | , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | An adhesive composition for a polarizing plate is adapted to exhibit a variation in relaxation modulus of an adhesive layer in a range of 75% to 95% before and after leaving the same at a temperature of −20° C. to 0° C. for 4 hours, such that it is possible to remarkably improve thermal-shock durability of the polarizing plate, and suppress a damage of the polarizing plate in a thermal-shock durability test, while maintaining excellent adhesiveness. |
---|