Polyethylene compositions and methods of making and using same

A polyolefin having a density of greater than about 0.930 g/ml which when extruded at a temperature in the range of from about 590° F. to about 645° F. and then coated onto a substrate at a rate of from about 300 ft/min to about 1000 ft/min has an edge weave of from about 0 in/side to about 2.5 in/s...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: Frey, Kelly, Sukhadia, Ashish M, Tso, Chung, Cruz, Carlos A, Yang, Qing, Yu, Youlu, McDaniel, Max P, Barr, Jared L, Hert, Daniel G, Fisher, William, Bridendolph, Bill, Rutledge-Ryal, Brandy, Inn, Yongwoo
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:A polyolefin having a density of greater than about 0.930 g/ml which when extruded at a temperature in the range of from about 590° F. to about 645° F. and then coated onto a substrate at a rate of from about 300 ft/min to about 1000 ft/min has an edge weave of from about 0 in/side to about 2.5 in/side and a neck-in of less than about 3.0 in/side.