Protective coating for metal surfaces
A method for heating or cooling a carbon containing reducing gas having a carbon monoxide content of at least 0.5 vol %, wherein the gas is heated to a temperature of at least 400° C. or wherein the gas is cooled from a temperature exceeding 400° C., wherein the gas is passed along a surface of a he...
Gespeichert in:
Hauptverfasser: | , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | A method for heating or cooling a carbon containing reducing gas having a carbon monoxide content of at least 0.5 vol %, wherein the gas is heated to a temperature of at least 400° C. or wherein the gas is cooled from a temperature exceeding 400° C., wherein the gas is passed along a surface of a heating or cooling unit having a heat conductive metal or metal alloy body and a protective layer, which protective layer provides said surface, and which protective layer is made from a coating composition including colloidal amorphous silicate and crystalline oxide particles. |
---|