METHOD FOR MANUFACTURING PIPES OF AUSTENITIC STEELS
A method for manufacturing pipes of austenitic steels includes heating pre-drilled pieces, expansion thereof, heating the obtained hollow pipes, pressing, further cooling in water. Heating the billets prior to expansion is carried out to a temperature, which is determined by the formula. Heating the...
Gespeichert in:
Hauptverfasser: | , , , , , , , , |
---|---|
Format: | Patent |
Sprache: | eng ; rus ; ukr |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | A method for manufacturing pipes of austenitic steels includes heating pre-drilled pieces, expansion thereof, heating the obtained hollow pipes, pressing, further cooling in water. Heating the billets prior to expansion is carried out to a temperature, which is determined by the formula. Heating the hollow pipes before pressing is carried to a temperature, which is by 1.017-1.034 times higher than the heating temperature of the billets prior expansion.
Способ изготовления труб из аустенитных сталей включает нагрев предварительно просверленных заготовок, их экспандирование, подогрев полученных гильз, прессование, дальнейшее охлаждение в воде. Нагрев заготовок перед экспандированием осуществляют до температуры, которую определяют по формуле. Подогрев гильз перед прессованием осуществляют до температуры, которая в 1,017-1,034 раза больше, чем температура нагрева заготовок перед экспандированием.
Спосіб виготовлення труб із аустенітних сталей включає нагрівання попередньо свердлених заготовок, їхнє експандування, підігрівання отриманих гільз, пресування, подальше охолодження в воді. Нагрівання заготовок перед експандуванням здійснюють до температури, яку визначають за формулою. Підігрівання гільз перед пресуванням здійснюють до температури, яка в 1,017-1,034 разу більша, ніж температура нагрівання заготовок перед експандуванням. |
---|