METHOD FOR OBTAINING COATING ON THE SURFACE OF METAL ARTICLES

Method for obtaining coating on the surface of metal articles preferably of heat and protective purpose, which method comprises thermal treatment in the following mode: keeping for 15 min. at the temperature of coating application of 125-135 DEGREE C, further not less than 25 min. at the temperature...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: KOROLIOV VOLODYMYR HEORHIIOVYCH, KALASHNIKOV MYKOLA OLEKSANDROVYCH, BALITSKYI IVAN PETROVYCH, KRASNIKOV OLEKSII IVANOVYCH
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Method for obtaining coating on the surface of metal articles preferably of heat and protective purpose, which method comprises thermal treatment in the following mode: keeping for 15 min. at the temperature of coating application of 125-135 DEGREE C, further not less than 25 min. at the temperature of 154-156 DEGREE C and not less than 30 min. in achieving the temperature of polymerization during the last cycle.