METHOD FOR PREPARATION OF SLURRY-COAL HYDROSUSPENSION

A slurry-coal hydrosuspension is prepared by preliminary wetting the slurry coal at weight ratio of water: slurry of 1:(5-10), keeping thereof wetted for 0.5-10.0 hours, wet milling in the ball or rod mill in the presence of additive of lignosulfonate and sodium hydroxide, which are taken at a weigh...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: ZAVHORODNII VOLODYMYR ANDRIIOVYCH, YEHURNOV OLEKSANDR IVANOVYCH, MAKAROV ANATOLII SEMENOVYCH, KOKHANOK OLEKSANDR LEONIDOVYCH
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:A slurry-coal hydrosuspension is prepared by preliminary wetting the slurry coal at weight ratio of water: slurry of 1:(5-10), keeping thereof wetted for 0.5-10.0 hours, wet milling in the ball or rod mill in the presence of additive of lignosulfonate and sodium hydroxide, which are taken at a weight ratio of dry reagents of 3:1, and additive is introduced at an amount of 1% for solid phase mass.