A refractory concrete composition

A refractory concrete composition intended preferably for making solid linings of heat units contains 79.5-84.6 % by weight of chamotte filling material and 15.4-20.5 % by weight of binding material. As binding material it contains finely dispersed mix of high-aliminous cement and chamotte taken at...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: Soloshenko Liudmyla Mykolaivna, Scherbak Liudmyla Mykhailivna, Sviatolutska Vira Mykhailivna, Babkina Lina Oleksiivna
Format: Patent
Sprache:eng ; rus ; ukr
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:A refractory concrete composition intended preferably for making solid linings of heat units contains 79.5-84.6 % by weight of chamotte filling material and 15.4-20.5 % by weight of binding material. As binding material it contains finely dispersed mix of high-aliminous cement and chamotte taken at a ratio between 1.0:0.4 and 1.3:0.6. It provides a high resistance of calcinations furnaces. Огнеупорная бетонная смесь, предназначенная преимущественно для изготовления монолитных футеровок тепловых агрегатов, содержит 79,5-84,6 масс. % шамотного заполнителя и 15,4-20,5 масс. % вяжущего. Как вяжущее она содержит тонкомолотую смесь высокоглиноземистого цемента и шамота, взятых в соотношении от 1,0:0,4 до 1,3:0,6. Обеспечивает повышенную стойкость футеровки печей кальцинации. Вогнетривка бетонна суміш, яка призначена переважно для виготовлення монолітних футерівок теплових агрегатів, містить 79,5-84,6 мас. % шамотного заповнювача і 15,4-20,5 мас. % в'яжучого. Як в'яжуче вона містить тонкомелену суміш високоглиноземистого цементу і шамоту, узятих у співвідношенні від 1,0:0,4 до 1,3:0,6. Забезпечує підвищену стійкість футерівки печей кальцинації.