METHOD WOR WASHING THE HEARTH OF A BLAST-FURNACE
Method for washing the hearth of a blast-furnace includes loading to the furnace washing charge as welding slag, iron ore, manganese ore, fluor-spar, and after it comes to the hearth feeding is terminated for 15-120 minutes, for regeneration additives in 5-10 minutes after opening the cast-iron tap...
Gespeichert in:
Hauptverfasser: | , , , , , , , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | Method for washing the hearth of a blast-furnace includes loading to the furnace washing charge as welding slag, iron ore, manganese ore, fluor-spar, and after it comes to the hearth feeding is terminated for 15-120 minutes, for regeneration additives in 5-10 minutes after opening the cast-iron tap hole. In feeding the preliminary loading of washing charge mass of limestone is decreased. |
---|