METHOD FOR REGENERATION OF ZEOLITE-MORDENITE
The method for regeneration of zeolite-mordenite consists in removal of water and organic compounds from the zeolite channels. Steam or carbonic acid superheated at the temperature of 220-245 DEGREE C for 120-160 minutes is used as a sorbent.