METHOD FOR REPAIR OF FUEL TANKS OF HELICOPTERS

A method for repair of fuel tanks of helicopters, according to which following operations are performed: removal of a fuel tank from airframe, determination of damaged areas of on its body, removal of paint and traces of possible corrosion on the outside of body of fuel tank in damaged areas and aro...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: NEMCHYN OLEKSANDR FEDOROVYCH, MYKHAILENKO VOLODYMYR PAVLOVYCH, ZUBKO MYKOLA OLEKSANDROVYCH, BUTSAN ANATOLII OLEKSIIOVYCH, SEREDOKHIN VOLODYMYR OLEKSIIOVYCH, MYKHAILYTSKA NATALIA VALENTYNIVNA
Format: Patent
Sprache:eng ; rus ; ukr
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator NEMCHYN OLEKSANDR FEDOROVYCH
MYKHAILENKO VOLODYMYR PAVLOVYCH
ZUBKO MYKOLA OLEKSANDROVYCH
BUTSAN ANATOLII OLEKSIIOVYCH
SEREDOKHIN VOLODYMYR OLEKSIIOVYCH
MYKHAILYTSKA NATALIA VALENTYNIVNA
description A method for repair of fuel tanks of helicopters, according to which following operations are performed: removal of a fuel tank from airframe, determination of damaged areas of on its body, removal of paint and traces of possible corrosion on the outside of body of fuel tank in damaged areas and around them, manufacturing from an aluminum alloy of compensating patches with an overlap for each damage, degreasing the surface of tank and one of the sides of compensating patches, preparing a metal-polymer paste as a mixture of base and activator in the proportions and manner specified in the accompanying documentation for the set of components of metal-polymer paste, application of the prepared metal-polymer paste on the damaged areas and degreased sides of compensating patches, application of the compensating patches by side with deposited metal-polymer paste on appropriate damaged areas providing their firm adherence, removal, in case of need, of any excess paste by a solvent specified in the accompanying documentation for the set of components of metal-polymer paste, tightness control of fuel tank after curing and hardening of metal-polymer paste, preparing the repaired surfaces of body of fuel tank by grinding and priming for paint coating, application of paint coating, mounting of fuel tank on the airframe. The sheet of Al-Mg alloy with thickness of 0.5- is used as a material for compensating patches. After application of the compensatory patches on the damaged areas a pressure is created with loads on the compensating patches followed by application of vibration loads to the body of fuel tanks from 4 to 6 minutes after installation of the loads. Duration of application of vibration loads is inversely proportional to the size of through damages of fuel tank body. Sinusoidal vibrations with a frequency of (50 ± 5) Hz and acceleration amplitude of (0.03 ± 0.1) m/sare used as vibratory loads on the body of fuel tanks. Спосіб ремонту паливних баків гелікоптерів, за яким паливний бак демонтують з планера гелікоптера, визначають місця пошкоджень на його корпусі, видаляють лакофарбові покриття та сліди можливої корозії на зовнішній стороні корпусу паливного бака в місцях пошкоджень та навколо них, готують з алюмінієвого сплаву компенсуючі латки з напустком для кожного ушкодження, обезжирюють оброблену поверхню паливного бака та одну з сторін компенсуючих латок, готують металополімерну пасту як суміш основи та активатора у пропорціях та порядку, що вказані в супр
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_UA57919UU</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>UA57919UU</sourcerecordid><originalsourceid>FETCH-epo_espacenet_UA57919UU3</originalsourceid><addsrcrecordid>eNrjZNDzdQ3x8HdRcPMPUghyDXD0DFLwd1NwC3X1UQhx9PMOBvE8XH08nf0DQlyDgnkYWNMSc4pTeaE0N4Ocm2uIs4duakF-fGpxQWJyal5qSXyoo6m5paFlaKgxQQUA-TQkzQ</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METHOD FOR REPAIR OF FUEL TANKS OF HELICOPTERS</title><source>esp@cenet</source><creator>NEMCHYN OLEKSANDR FEDOROVYCH ; MYKHAILENKO VOLODYMYR PAVLOVYCH ; ZUBKO MYKOLA OLEKSANDROVYCH ; BUTSAN ANATOLII OLEKSIIOVYCH ; SEREDOKHIN VOLODYMYR OLEKSIIOVYCH ; MYKHAILYTSKA NATALIA VALENTYNIVNA</creator><creatorcontrib>NEMCHYN OLEKSANDR FEDOROVYCH ; MYKHAILENKO VOLODYMYR PAVLOVYCH ; ZUBKO MYKOLA OLEKSANDROVYCH ; BUTSAN ANATOLII OLEKSIIOVYCH ; SEREDOKHIN VOLODYMYR OLEKSIIOVYCH ; MYKHAILYTSKA NATALIA VALENTYNIVNA</creatorcontrib><description>A method for repair of fuel tanks of helicopters, according to which following operations are performed: removal of a fuel tank from airframe, determination of damaged areas of on its body, removal of paint and traces of possible corrosion on the outside of body of fuel tank in damaged areas and around them, manufacturing from an aluminum alloy of compensating patches with an overlap for each damage, degreasing the surface of tank and one of the sides of compensating patches, preparing a metal-polymer paste as a mixture of base and activator in the proportions and manner specified in the accompanying documentation for the set of components of metal-polymer paste, application of the prepared metal-polymer paste on the damaged areas and degreased sides of compensating patches, application of the compensating patches by side with deposited metal-polymer paste on appropriate damaged areas providing their firm adherence, removal, in case of need, of any excess paste by a solvent specified in the accompanying documentation for the set of components of metal-polymer paste, tightness control of fuel tank after curing and hardening of metal-polymer paste, preparing the repaired surfaces of body of fuel tank by grinding and priming for paint coating, application of paint coating, mounting of fuel tank on the airframe. The sheet of Al-Mg alloy with thickness of 0.5- is used as a material for compensating patches. After application of the compensatory patches on the damaged areas a pressure is created with loads on the compensating patches followed by application of vibration loads to the body of fuel tanks from 4 to 6 minutes after installation of the loads. Duration of application of vibration loads is inversely proportional to the size of through damages of fuel tank body. Sinusoidal vibrations with a frequency of (50 ± 5) Hz and acceleration amplitude of (0.03 ± 0.1) m/sare used as vibratory loads on the body of fuel tanks. Спосіб ремонту паливних баків гелікоптерів, за яким паливний бак демонтують з планера гелікоптера, визначають місця пошкоджень на його корпусі, видаляють лакофарбові покриття та сліди можливої корозії на зовнішній стороні корпусу паливного бака в місцях пошкоджень та навколо них, готують з алюмінієвого сплаву компенсуючі латки з напустком для кожного ушкодження, обезжирюють оброблену поверхню паливного бака та одну з сторін компенсуючих латок, готують металополімерну пасту як суміш основи та активатора у пропорціях та порядку, що вказані в супровідній документації на набір компонентів металополімерної пасти, наносять приготовлену металополімерну пасту на місця пошкоджень та обезжирені сторони компенсуючих латок, накладають компенсуючі латки стороною з нанесеною металополімерною пастою на відповідні місця ушкоджень та забезпечують їх щільне прилягання, в разі необхідності надлишки пасти знімають за допомогою розчинника, вказаного в супровідній документації на набір компонентів металополімерної пасти, після полімеризації та затвердіння металополімерної пасти перевіряють паливний бак на герметичність, ремонтовані поверхні корпусу паливного бака шляхом шліфовки та ґрунтування готують до нанесення лакофарбового покриття, наносять лакофарбове покриття, монтують паливний бак на планер гелікоптера. Як матеріал компенсуючих латок використовують лист сплаву АМц товщиною 0,5-. Після накладення компенсуючих латок на місця пошкоджень за допомогою тягарів створюють тиск на компенсуючі латки, протягом від 4 до 6 хвилин після встановлення тягарів до корпусу паливних баків застосовують вібраційні навант�</description><language>eng ; rus ; ukr</language><subject>COMBINED OPERATIONS ; MACHINE TOOLS ; METAL-WORKING NOT OTHERWISE PROVIDED FOR ; OTHER WORKING OF METAL ; PERFORMING OPERATIONS ; TRANSPORTING ; UNIVERSAL MACHINE TOOLS</subject><creationdate>2011</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20110310&amp;DB=EPODOC&amp;CC=UA&amp;NR=57919U$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20110310&amp;DB=EPODOC&amp;CC=UA&amp;NR=57919U$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>NEMCHYN OLEKSANDR FEDOROVYCH</creatorcontrib><creatorcontrib>MYKHAILENKO VOLODYMYR PAVLOVYCH</creatorcontrib><creatorcontrib>ZUBKO MYKOLA OLEKSANDROVYCH</creatorcontrib><creatorcontrib>BUTSAN ANATOLII OLEKSIIOVYCH</creatorcontrib><creatorcontrib>SEREDOKHIN VOLODYMYR OLEKSIIOVYCH</creatorcontrib><creatorcontrib>MYKHAILYTSKA NATALIA VALENTYNIVNA</creatorcontrib><title>METHOD FOR REPAIR OF FUEL TANKS OF HELICOPTERS</title><description>A method for repair of fuel tanks of helicopters, according to which following operations are performed: removal of a fuel tank from airframe, determination of damaged areas of on its body, removal of paint and traces of possible corrosion on the outside of body of fuel tank in damaged areas and around them, manufacturing from an aluminum alloy of compensating patches with an overlap for each damage, degreasing the surface of tank and one of the sides of compensating patches, preparing a metal-polymer paste as a mixture of base and activator in the proportions and manner specified in the accompanying documentation for the set of components of metal-polymer paste, application of the prepared metal-polymer paste on the damaged areas and degreased sides of compensating patches, application of the compensating patches by side with deposited metal-polymer paste on appropriate damaged areas providing their firm adherence, removal, in case of need, of any excess paste by a solvent specified in the accompanying documentation for the set of components of metal-polymer paste, tightness control of fuel tank after curing and hardening of metal-polymer paste, preparing the repaired surfaces of body of fuel tank by grinding and priming for paint coating, application of paint coating, mounting of fuel tank on the airframe. The sheet of Al-Mg alloy with thickness of 0.5- is used as a material for compensating patches. After application of the compensatory patches on the damaged areas a pressure is created with loads on the compensating patches followed by application of vibration loads to the body of fuel tanks from 4 to 6 minutes after installation of the loads. Duration of application of vibration loads is inversely proportional to the size of through damages of fuel tank body. Sinusoidal vibrations with a frequency of (50 ± 5) Hz and acceleration amplitude of (0.03 ± 0.1) m/sare used as vibratory loads on the body of fuel tanks. Спосіб ремонту паливних баків гелікоптерів, за яким паливний бак демонтують з планера гелікоптера, визначають місця пошкоджень на його корпусі, видаляють лакофарбові покриття та сліди можливої корозії на зовнішній стороні корпусу паливного бака в місцях пошкоджень та навколо них, готують з алюмінієвого сплаву компенсуючі латки з напустком для кожного ушкодження, обезжирюють оброблену поверхню паливного бака та одну з сторін компенсуючих латок, готують металополімерну пасту як суміш основи та активатора у пропорціях та порядку, що вказані в супровідній документації на набір компонентів металополімерної пасти, наносять приготовлену металополімерну пасту на місця пошкоджень та обезжирені сторони компенсуючих латок, накладають компенсуючі латки стороною з нанесеною металополімерною пастою на відповідні місця ушкоджень та забезпечують їх щільне прилягання, в разі необхідності надлишки пасти знімають за допомогою розчинника, вказаного в супровідній документації на набір компонентів металополімерної пасти, після полімеризації та затвердіння металополімерної пасти перевіряють паливний бак на герметичність, ремонтовані поверхні корпусу паливного бака шляхом шліфовки та ґрунтування готують до нанесення лакофарбового покриття, наносять лакофарбове покриття, монтують паливний бак на планер гелікоптера. Як матеріал компенсуючих латок використовують лист сплаву АМц товщиною 0,5-. Після накладення компенсуючих латок на місця пошкоджень за допомогою тягарів створюють тиск на компенсуючі латки, протягом від 4 до 6 хвилин після встановлення тягарів до корпусу паливних баків застосовують вібраційні навант�</description><subject>COMBINED OPERATIONS</subject><subject>MACHINE TOOLS</subject><subject>METAL-WORKING NOT OTHERWISE PROVIDED FOR</subject><subject>OTHER WORKING OF METAL</subject><subject>PERFORMING OPERATIONS</subject><subject>TRANSPORTING</subject><subject>UNIVERSAL MACHINE TOOLS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2011</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZNDzdQ3x8HdRcPMPUghyDXD0DFLwd1NwC3X1UQhx9PMOBvE8XH08nf0DQlyDgnkYWNMSc4pTeaE0N4Ocm2uIs4duakF-fGpxQWJyal5qSXyoo6m5paFlaKgxQQUA-TQkzQ</recordid><startdate>20110310</startdate><enddate>20110310</enddate><creator>NEMCHYN OLEKSANDR FEDOROVYCH</creator><creator>MYKHAILENKO VOLODYMYR PAVLOVYCH</creator><creator>ZUBKO MYKOLA OLEKSANDROVYCH</creator><creator>BUTSAN ANATOLII OLEKSIIOVYCH</creator><creator>SEREDOKHIN VOLODYMYR OLEKSIIOVYCH</creator><creator>MYKHAILYTSKA NATALIA VALENTYNIVNA</creator><scope>EVB</scope></search><sort><creationdate>20110310</creationdate><title>METHOD FOR REPAIR OF FUEL TANKS OF HELICOPTERS</title><author>NEMCHYN OLEKSANDR FEDOROVYCH ; MYKHAILENKO VOLODYMYR PAVLOVYCH ; ZUBKO MYKOLA OLEKSANDROVYCH ; BUTSAN ANATOLII OLEKSIIOVYCH ; SEREDOKHIN VOLODYMYR OLEKSIIOVYCH ; MYKHAILYTSKA NATALIA VALENTYNIVNA</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_UA57919UU3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; rus ; ukr</language><creationdate>2011</creationdate><topic>COMBINED OPERATIONS</topic><topic>MACHINE TOOLS</topic><topic>METAL-WORKING NOT OTHERWISE PROVIDED FOR</topic><topic>OTHER WORKING OF METAL</topic><topic>PERFORMING OPERATIONS</topic><topic>TRANSPORTING</topic><topic>UNIVERSAL MACHINE TOOLS</topic><toplevel>online_resources</toplevel><creatorcontrib>NEMCHYN OLEKSANDR FEDOROVYCH</creatorcontrib><creatorcontrib>MYKHAILENKO VOLODYMYR PAVLOVYCH</creatorcontrib><creatorcontrib>ZUBKO MYKOLA OLEKSANDROVYCH</creatorcontrib><creatorcontrib>BUTSAN ANATOLII OLEKSIIOVYCH</creatorcontrib><creatorcontrib>SEREDOKHIN VOLODYMYR OLEKSIIOVYCH</creatorcontrib><creatorcontrib>MYKHAILYTSKA NATALIA VALENTYNIVNA</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>NEMCHYN OLEKSANDR FEDOROVYCH</au><au>MYKHAILENKO VOLODYMYR PAVLOVYCH</au><au>ZUBKO MYKOLA OLEKSANDROVYCH</au><au>BUTSAN ANATOLII OLEKSIIOVYCH</au><au>SEREDOKHIN VOLODYMYR OLEKSIIOVYCH</au><au>MYKHAILYTSKA NATALIA VALENTYNIVNA</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METHOD FOR REPAIR OF FUEL TANKS OF HELICOPTERS</title><date>2011-03-10</date><risdate>2011</risdate><abstract>A method for repair of fuel tanks of helicopters, according to which following operations are performed: removal of a fuel tank from airframe, determination of damaged areas of on its body, removal of paint and traces of possible corrosion on the outside of body of fuel tank in damaged areas and around them, manufacturing from an aluminum alloy of compensating patches with an overlap for each damage, degreasing the surface of tank and one of the sides of compensating patches, preparing a metal-polymer paste as a mixture of base and activator in the proportions and manner specified in the accompanying documentation for the set of components of metal-polymer paste, application of the prepared metal-polymer paste on the damaged areas and degreased sides of compensating patches, application of the compensating patches by side with deposited metal-polymer paste on appropriate damaged areas providing their firm adherence, removal, in case of need, of any excess paste by a solvent specified in the accompanying documentation for the set of components of metal-polymer paste, tightness control of fuel tank after curing and hardening of metal-polymer paste, preparing the repaired surfaces of body of fuel tank by grinding and priming for paint coating, application of paint coating, mounting of fuel tank on the airframe. The sheet of Al-Mg alloy with thickness of 0.5- is used as a material for compensating patches. After application of the compensatory patches on the damaged areas a pressure is created with loads on the compensating patches followed by application of vibration loads to the body of fuel tanks from 4 to 6 minutes after installation of the loads. Duration of application of vibration loads is inversely proportional to the size of through damages of fuel tank body. Sinusoidal vibrations with a frequency of (50 ± 5) Hz and acceleration amplitude of (0.03 ± 0.1) m/sare used as vibratory loads on the body of fuel tanks. Спосіб ремонту паливних баків гелікоптерів, за яким паливний бак демонтують з планера гелікоптера, визначають місця пошкоджень на його корпусі, видаляють лакофарбові покриття та сліди можливої корозії на зовнішній стороні корпусу паливного бака в місцях пошкоджень та навколо них, готують з алюмінієвого сплаву компенсуючі латки з напустком для кожного ушкодження, обезжирюють оброблену поверхню паливного бака та одну з сторін компенсуючих латок, готують металополімерну пасту як суміш основи та активатора у пропорціях та порядку, що вказані в супровідній документації на набір компонентів металополімерної пасти, наносять приготовлену металополімерну пасту на місця пошкоджень та обезжирені сторони компенсуючих латок, накладають компенсуючі латки стороною з нанесеною металополімерною пастою на відповідні місця ушкоджень та забезпечують їх щільне прилягання, в разі необхідності надлишки пасти знімають за допомогою розчинника, вказаного в супровідній документації на набір компонентів металополімерної пасти, після полімеризації та затвердіння металополімерної пасти перевіряють паливний бак на герметичність, ремонтовані поверхні корпусу паливного бака шляхом шліфовки та ґрунтування готують до нанесення лакофарбового покриття, наносять лакофарбове покриття, монтують паливний бак на планер гелікоптера. Як матеріал компенсуючих латок використовують лист сплаву АМц товщиною 0,5-. Після накладення компенсуючих латок на місця пошкоджень за допомогою тягарів створюють тиск на компенсуючі латки, протягом від 4 до 6 хвилин після встановлення тягарів до корпусу паливних баків застосовують вібраційні навант�</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; rus ; ukr
recordid cdi_epo_espacenet_UA57919UU
source esp@cenet
subjects COMBINED OPERATIONS
MACHINE TOOLS
METAL-WORKING NOT OTHERWISE PROVIDED FOR
OTHER WORKING OF METAL
PERFORMING OPERATIONS
TRANSPORTING
UNIVERSAL MACHINE TOOLS
title METHOD FOR REPAIR OF FUEL TANKS OF HELICOPTERS
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-18T16%3A38%3A40IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=NEMCHYN%20OLEKSANDR%20FEDOROVYCH&rft.date=2011-03-10&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EUA57919UU%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true