PROCESS FOR THE PREPARATION OF FLUOR APATITE
A process for the preparation of fluor apatite comprises the preparation of furnace charge, its thermal treatment and separation of base product. The furnace charge is prepared by means of mixing of metaphosphate or orthophosphate of alkali metal, namely Na3PO4 with CaF2. Thermal treatment is carrie...
Gespeichert in:
Hauptverfasser: | , , , , |
---|---|
Format: | Patent |
Sprache: | eng ; rus ; ukr |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | A process for the preparation of fluor apatite comprises the preparation of furnace charge, its thermal treatment and separation of base product. The furnace charge is prepared by means of mixing of metaphosphate or orthophosphate of alkali metal, namely Na3PO4 with CaF2. Thermal treatment is carried out in melt of eutectic NaNO3 - KNO3 at temperature of 250-350 °C and mass ratio of base product:eutectic, equal to 1:1.
Способ получения фторапатита включает приготовление шихты, ее термообработку и отделение целевого продукта. Шихту готовят путем смешивания метафосфата или ортофосфата щелочного металла, а именно Na3PO4 с CaF2. Термообработку осуществляют в расплаве эвтектики NaNO3 - KNO3 при температуре 250-350 °С и массовом соотношении готовый продукт: эвтектика, равном 1:1.
Спосіб одержання фтороапатиту включає приготування шихти, її термообробку та відокремлення цільового продукту. Шихту готують шляхом змішування метафосфату або ортофосфату лужного металу, а саме Na3PO4 з CaF2. Термообробку здійснюють в розтопі евтектики NaNO3 - KNO3 при температурі 250-350 °С і масовому співвідношенні готовий продукт:евтектика, що дорівнює 1:1. |
---|