METHOD FOR APPLICATION OF DIFFUSION BORON-CHROMIUM COATINGS

Method for application of diffusion boron-chromium coatings on steels consists in diffuse saturation of the articles in the melt of fluid metal with the coating elements introduced in it. Saturation is made at 850-950 ° and is kept at this temperature during 5-8 hours in lithium melt. Boron and chro...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: RUDKOVSKYI YEVHEN MARIANOVYCH, RATSKA NADIA BOHDANIVNA, VASYLIV KHRYSTYNA BRONISLAVIVNA, SHYROKOV VOLODYMYR VOLODYMYROVYCH, ARENDAR LIUBOMYR ANATOLIIOVYCH
Format: Patent
Sprache:eng ; rus ; ukr
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Method for application of diffusion boron-chromium coatings on steels consists in diffuse saturation of the articles in the melt of fluid metal with the coating elements introduced in it. Saturation is made at 850-950 ° and is kept at this temperature during 5-8 hours in lithium melt. Boron and chrome oxide are used as saturation elements. Способ нанесения диффузных борохромовых покрытий на сталях заключается в диффузном насыщении изделий в расплаве легкоплавкого металла, в который введены элементы покрытия. Насыщение выполняют при 850-950 °С и выдерживают при этой температуре 5-8 ч. в расплаве лития. Как насыщающие элементы используют бор и оксид хрома. Спосіб нанесення дифузійних борохромових покрить на сталях полягає в дифузійному насиченні виробів в розплаві легкоплавкого металу, у який введено елементи покриття. Насичення виконують при 850-950 °С і витримують при цій температури 5-8 год. в розплаві літію. Як насичуючі елементи використовують бор і оксид хрому.