PROCESS FOR THE PREPARATION OF MODIFIED EPOXY COMPOSITE COATING

A process for the preparation of modified epoxy composite coating consists in treatment of adhesive layer by ultrasound and thermal treatment at =323±2 for τ=1.5-2.0 hours. Thereafter preliminarily treated in constant magnetic field and modified with electrodischarge machining surface layer is appli...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: DOBROTVOR IHOR HRYHOROVYCH, CHYKHIRA IHOR VIKTOROVYCH, ZOLOTYI ROMAN ZAKHARIIOVYCH, BUKETOV ANDRII VIKTOROVYCH
Format: Patent
Sprache:eng ; rus ; ukr
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:A process for the preparation of modified epoxy composite coating consists in treatment of adhesive layer by ultrasound and thermal treatment at =323±2 for τ=1.5-2.0 hours. Thereafter preliminarily treated in constant magnetic field and modified with electrodischarge machining surface layer is applied with subsequent coating curing at temperature of =293-298 for τ=72-76 hours. Способ получения модифицированного эпоксикомпозитного покрытия, при котором адгезионный слой предварительно обрабатывают ультразвуком и термообрабатывают при температуре Т=323±2 К на протяжении τ=1,5-2,0 ч., потом наносят предварительно обработанный в постоянном магнитном поле, а в дальнейшем - модифицированный электроискровой обработкой поверхностный слой с последующим твердением покрытия при температуре Т=293-298 К на протяжении τ=72-76 ч. Спосіб отримання модифікованого епоксикомпозитного покриття, при якому адгезійний шар попередньо обробляють ультразвуком і термообробляють при температурі Т=323±2 К протягом τ=1,5-2,0 год., потім наносять попередньо оброблений у постійному магнітному полі, а у подальшому - модифікований електроіскровим обробленням поверхневий шар з наступним твердненням покриття при температурі Т=293-298 К протягом τ=72-76 год.